Coal tar pitch rheology is a key design parameter that controls the microstructure and performance of pitch-bonded doloma refractories. Palmitic acid was introduced for the first time as a rheological modifier, with the optimum at 6 wt.%. At this level, the modified binder shows simultaneous reductions in softening point , viscosity and surface tension, while residual carbon decreases only slightly. These improvements promote better particle packing and binder distribution, increasing bulk density from 2.72 to 2.91 g·cm⁻³ and decreasing apparent porosity from 10.8% to 5.9%. Consequently, cold crushing strength rises by ~30%. Scanning Electron Microscopy (SEM) micrographs reveals a refined microstructure with finer pores and enhanced interparticle bonding, yielding a 33% improvement in thermal shock resistance (modulus of rupture, MOR ratio). The 6 wt.% sample also shows a 43% reduction in moisture uptake after 10 days at 25 °C and 95% Relative humidity (RH), confirming superior hydration resistance. These findings link binder rheology, microstructure, and performance, showing that engineering the rheology of a carbonaceous binder offers a new design path for optimizing basic refractories without changing manufacturing route.